Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 26.0 g/m²/day | 1.67 g/100 in²/day | 38°C, 90% RH; 25um; ASTM E96 |
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a.. |
|||
Water Vapor Transmission | 26.0 g/m²/day | 1.67 g/100 in²/day | ASTM E96 Procedure E |
DuPont Teijin Films Mylar® HS Polyester Film, 80 Gauge (20 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe.. |