Vapor Pressure 0.00540 bar
4.05 torr
BASF Butyl Acrylate
Formula: C7H12O2CAS: 141-32-2Description: Acrylic acid ester, for manufacturing polymers and for use as a feedstock for syntheses.Applications: Butyl acrylate forms homopolymers and copolymers. Copo..