Physical Properties Metric English Comments
Vapor Pressure 4.00e-7 bar

@Temperature 25.0 °C
0.000300 torr

@Temperature 77.0 °F
BASF Lupranate® 227 Isocyanate
Description: Lupranate® 227 Isocyanate is a liquid, modified blend product based on isomers of diphenylmethane diisocyanate (MDI). This product has good storage stability at room temperature and of..
Vapor Pressure 4.00e-7 bar

@Temperature 25.0 °C
0.000300 torr

@Temperature 77.0 °F
BASF Lupranate® 265 Isocyanate
Description: Lupranate® 265 Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate 265 Isocyanate is used in the i..
Vapor Pressure 4.00e-7 bar

@Temperature 25.0 °C
0.000300 torr

@Temperature 77.0 °F
BASF Lupranate® MI Isocyanate
Description: Lupranate® MI Isocyanate is pure diphenylmethane diisocyanate containing a higher amount of 2,4´ isomer than Lupranate M Isocyanate or Lupranate MS Isocyanate. Lupranate MI Isocyanate..
Vapor Pressure 4.00e-7 bar

@Temperature 25.0 °C
0.000300 torr

@Temperature 77.0 °F
BASF Lupranate® MT Isocyanate
Description: Lupranate® MT Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate® MT Isocyanate is used in the ..
Vapor Pressure 4.00e-7 bar

@Temperature 25.0 °C
0.000300 torr

@Temperature 77.0 °F
BASF Lupranate® MTD Isocyanate
Description: Lupranate® MTD Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate® MTD Isocyanate is used in the..
Vapor Pressure 4.00e-7 bar

@Temperature 25.0 °C
0.000300 torr

@Temperature 77.0 °F
BASF Lupranate® 234 Isocyanate
Description: Lupranate® 234 Isocyanate is a low functionality (approximately 2.3) low viscosity polymeric MDI with high 2,4’-MDI isomer content. Lupranate® 234 Isocyanate exhibits excellent low t..
Vapor Pressure 4.00e-7 bar

@Temperature 25.0 °C
0.000300 torr

@Temperature 77.0 °F
BASF Lupranate® 241 Isocyanate
Description: Lupranate® 241 Isocyanate is a low functionality (approximately 2.3) low viscosity polymeric MDI with high2,4’-MDI isomer content. Lupranate® 241 Isocyanate exhibits excellent low t..
Vapor Pressure 4.00e-7 bar

@Temperature 25.0 °C
0.000300 torr

@Temperature 77.0 °F
BASF Lupranate® 78 Isocyanate
Description: Lupranate® 78 Isocyanate is a polymeric MDI with a functionality of approximately 2.3. This product exhibits excellent low temperature stability. Lupranate 78 Isocyanate will remain a ..
Vapor Pressure 4.00e-7 bar

@Temperature 25.0 °C
0.000300 torr

@Temperature 77.0 °F
BASF Lupranate® 81 Isocyanate
Description: Lupranate® 81 Isocyanate is a carbodiimide modified pure MDI with a higher 2,4’-isomer content and a functionality of approximately 2.1. Lupranate 81 Isocyanate exhibits good low temp..
Vapor Pressure 4.00e-7 bar

@Temperature 25.0 °C
0.000300 torr

@Temperature 77.0 °F
BASF Lupranate® M Isocyanate
Description: Lupranate® M Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate M Isocyanate is used in the isoc..