Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | <= 1.33e-8 bar | <= 0.0000100 torr | |
Dow ISONATE™ 143L Modified MDI ISONATE™ 143 is a polycarbodiimide-modified diphenylmethane diisocyanate. Liquid at room temperature, this product has a low viscosity and good storage stability down to 75°F. The polycarbodiimi.. |
|||
Vapor Pressure | <= 1.33e-8 bar | <= 0.0000100 torr | |
Dow ISONATE™ 240 MDI Prepolymer ISONATE™ 240 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with a high molecular weight polyester polyol, resulting in a material with good.. |
|||
Vapor Pressure | <= 1.33e-8 bar | <= 0.0000100 torr | |
Dow ISONATE™ 181 MDI Prepolymer ISONATE™ 181 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with sufficient glycol to allow easy handling down to 80°F. This medium-viscos.. |
|||
Vapor Pressure | <= 1.33e-8 bar | <= 0.0000100 torr | |
Dow PAPI™ 20 Polymeric MDI PAPI™ 20 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality value of 3.2 and high viscosity result in highly rigid foams. This product is design.. |
|||
Vapor Pressure | <= 1.33e-8 bar | <= 0.0000100 torr | |
Dow PAPI™ 580 N Polymeric MDI PAPI™ 580 N polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has high functionality (value of 3.0) and relatively high viscosity. Recommended for use in polyi.. |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 224 Isocyanate Description: Lupranate® 224 is a special medium viscosity polymeric MDI containing a high amount of 2,4'-diphenylmethane diisocyanate. The high 2,4'-MDI content will allow for better flow and lon.. |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 245 Isocyanate Description: Lupranate® 245 Isocyanate is a low viscosity polymeric diphenylmethane diisocyanate (polymeric MDI) containing a very high amount of monomeric diphenylmethane diisocyanate (pure MDI)In.. |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 279 Isocyanate Description: Lupranate® 279 Isocyanate is a 14% free-NCO prepolymer based on monomeric MDI chemistry. Lupranate 279 Isocyanate provides the lengthened open-time and high elongation desired in appli.. |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 3164T Isocyanate Description: Lupranate® 3164T Isocyanate is a low viscosity polymeric MDI containing a high amount of diphenylmethane diisocyanate (monomeric MDI).Information provided by BASF |
|||
Vapor Pressure | <= 1.33e-8 bar @Temperature 25.0 °C |
<= 0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 5020 Isocyanate Description: Lupranate® 5020 Isocyanate is a low free-NCO prepolymer based on pure MDI. The 9.5% free-NCO of Lupranate® 5020 Isocyanate lends itself to one-component applications, such as but not .. |
|||
Vapor Pressure | <= 1.33e-8 bar @Temperature 25.0 °C |
<= 0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 5030 Isocyanate Description: Lupranate® 5030 Isocyanate is a liquid urethane modified diphenylmethane diisocyanate. Lupranate 5030 Isocyanate is used in conjunction with high molecular weight polyester or polyethe.. |
|||
Vapor Pressure | <= 1.33e-8 bar @Temperature 25.0 °C |
<= 0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 5050 Isocyanate Description: Lupranate® 5050 Isocyanate is a prepolymer based on a modified, pure MDI. The intermediate free-NCO and slightly enhanced functionality of Lupranate 5050 isocyanate has benefited the f.. |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 5100 Isocyanate Description: Lupranate® 5100 Isocyanate is an isocyanate blend of monomeric and polymeric MDI. Typical use is for flexible slab stock and molded Visco-Elastic memory foams.Information provided by B.. |
|||
Vapor Pressure | <= 1.33e-8 bar @Temperature 25.0 °C |
<= 0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 5140 Isocyanate Description: Lupranate® 5140 Isocyanate is a prepolymer based on a modified, pure MDI. The intermediate free-NCO and enhanced functionality of Lupranate 5140 isocyanate has benefited the formulatio.. |
|||
Vapor Pressure | <= 1.33e-8 bar @Temperature 25.0 °C |
<= 0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® MM103 Isocyanate Modified MDI Description: Lupranate® MM103 is a liquid carbodiimide modified 4,4’-diphenylmethane diisocyanate. Lupranate MM103 serves as the isocyanate component in the production of microcellular urethane el.. |
|||
Vapor Pressure | <= 1.33e-8 bar @Temperature 25.0 °C |
<= 0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® MS Isocyanate Description: Lupranate® MS, a solid at room temperature, is essentially pure MDI and has a functionality of 2.0. Lupranate MS isocyanate is used in the isocyanate component for the preparation of e.. |
|||
Vapor Pressure | <= 1.33e-8 bar @Temperature 25.0 °C |
<= 0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 219 Isocyanate Modified MDI Description: Lupranate® 219 Isocyanate is a liquid carbodiimide modified 4,4’-diphenylmethane diisocyanate. Lupranate 219 Isocyanate is a light-colored alternative to Lupranate MM103 Isocyanate. .. |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 259 Isocyanate Description: Lupranate® 259 Isocyanate is a modified pure MDI. No 259 Isocyanate is applicable for use in all CASE applications.Information provided by BASF |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 266 Isocyanate Description: Lupranate® 266 Isocyanate is a low viscosity polymeric MDI containing a high amount of 2,4’ diphenylmethane diisocyanate. Lupranate® 266 Isocyanate displays excellent low temperatur.. |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 277 Isocyanate Description: Lupranate® 277 Isocyanate is a medium viscosity polymeric MDI isocyanateInformation provided by BASF |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 280 Isocyanate Description: Lupranate® 280 Isocyanate is an isocyanate blend of monomeric and polymeric MDI. Typical use is for flexible slab stock and molded Visco-Elastic memory foams.Information provided by BA.. |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 281 Isocyanate Description: Lupranate® 281 Isocyanate is a low viscosity polymeric diphenylmethane diisocyanate (polymeric MDI) containing a very high amount of monomeric diphenylmethane diisocyanate (2,4'-MDI an.. |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 5060 Isocyanate Description: Lupranate® 5060 Isocyanate is a low functional prepolymer based on monomeric MDI. Lupranate® 5060 isocyanate is suitable for use in a broad range of flexible, semi-flexible, and cast .. |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 5070 Isocyanate Description: Lupranate® 5070 Isocyanate is a low functional prepolymer based on pure MDI. Lupranate 5070 isocyanate is favored in solid elastomers and microcellular foams where the formulator desir.. |
|||
Vapor Pressure | <= 1.33e-8 bar @Temperature 25.0 °C |
<= 0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 5130 Isocyanate Description: Lupranate® 5130 Isocyanate has the combined characteristics of a liquid carbodiimidemodified isocyanate and a pure MDI prepolymer. The relatively low functionality and high free-NCO of.. |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 5220 Isocyanate Description: Lupranate® 5220 Isocyanate is a low viscosity polymeric MDI containing a high amount of diphenylmethane diisocyanate (monomeric MDI).Information provided by BASF |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® M20FB Isocyanate Description: Lupranate® M20FB is a polymeric MDI with a functionality of approximately 2.7. Lupranate® M20FB has faster reactivity than polymeric MDI currently used in the wood panel industry. Thi.. |
|||
Vapor Pressure | <= 1.33e-8 bar @Temperature 25.0 °C |
<= 0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® MS/264 Isocyanate Description: Lupranate® MS/264, a solid at room temperature, is essentially pure MDI and has a functionality of 2.0. Lupranate MS/264 isocyanate is used in the isocyanate component for the preparat.. |
|||
Vapor Pressure | <= 1.33e-8 bar @Temperature 25.0 °C |
<= 0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 5040 Isocyanate Description: Lupranate® 5040 Isocyanate has the combined characteristics of a liquid carbodiimidemodified isocyanate and a pure MDI prepolymer. The relatively low functionality and high free-NCO of.. |
|||
Vapor Pressure | 1.33e-8 bar @Temperature 25.0 °C |
0.00000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® LP30 Isocyanate Description: Lupranate® LP30 isocyanate is a solvent-free, modified pure diphenylmethane diisocyanate which is liquid at 30°C. It is designed to replace pure MDI in applications where it is desira.. |