Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | <= 1.33e-7 bar @Temperature 43.0 °C |
<= 0.000100 torr @Temperature 109 °F |
|
Dow ISONATE™ 125M Pure MDI ISONATE™ 125M is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This di-functional product is a key ingredient in preparing prepolymers f.. |
|||
Vapor Pressure | <= 1.33e-7 bar @Temperature 43.0 °C |
<= 0.000100 torr @Temperature 109 °F |
|
Dow ISONATE™ 125MDR Pure MDI ISONATE™ 125MDR is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This difunctional product is a key ingredient in preparing prepolymers .. |
|||
Vapor Pressure | <= 1.33e-7 bar @Temperature 43.0 °C |
<= 0.000100 torr @Temperature 109 °F |
|
Dow ISONATE™ 50 O,P` Pure MDI ISONATE™ 50 O,P` is a high ortho-para MDI designed for use in polyurethane adhesives, sealants, sports flooring, coatings, electrical encapsulants and flexible molded foams. ISONATE™ 50 O,P` offe.. |
|||
Vapor Pressure | <= 1.33e-7 bar @Temperature 25.0 °C |
<= 0.0000998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 5010 Isocyanate Description: Lupranate® 5010 Isocyanate is a prepolymer based on polymeric MDI.Information provided by BASF |