Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.1455 bar @Temperature 204 °C |
109.1 torr @Temperature 400 °F |
|
Duratherm 450 Paraffinic Heat Transfer Fluid Duratherm 450 - thermal fluid specifically engineered for applications requiring process heating and cooling efficiently between 30°F and 450°F. Economical and thermally stable, Duratherm 450 offe.. |