Polymer Property : Thickness = 749 microns Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Thickness 622 - 749 microns
24.5 - 29.5 mil
Overall
Arlon 51576R027 0.027" (0.686 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat..