Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 127 - 178 microns | 5.00 - 7.00 mil | Side 1 |
Arlon 19571R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 127 - 178 microns | 5.00 - 7.00 mil | Side 2 |
Arlon 19571R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 152 - 178 microns | 6.00 - 7.00 mil | with adhesive |
3M Scotchcal™ 3662 Graphic Film This is a 2-mil, durable, opaque film designed for making short term graphics that are applied to unsealed, outdoor, pedestrian traffic surfaces or selected smooth-to-rough wall surfaces. This film .. |
|||
Thickness | 152 - 178 microns | 6.00 - 7.00 mil | with adhesive |
3M Scotchcal™ 8662 Graphic Film This is a 2-mil, durable, opaque film designed for making short term graphics that are applied to unsealed, outdoor, pedestrian traffic surfaces or selected smooth-to-rough wall surfaces. This film .. |