Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 940 - 1090 microns | 37.0 - 43.0 mil | Overall |
Arlon 25122R040 0.040" (1.02 mm) Silicone Rubber on Laminated Fluoropolymer Film Appearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical values for the production material. The data should not be used to write, or in place of, material.. |
|||
Thickness | 940 - 1090 microns | 37.0 - 43.0 mil | Overall |
Arlon 940-07Rxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Thickness | 940 - 1090 microns | 37.0 - 43.0 mil | Overall |
Arlon 940-07Rxx-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Performance Advantages:Resists moisture, oxygen, and ozone to assure continuous high insulation values.Conforms smoothly when wr.. |
|||
Thickness | 940 - 1090 microns | 37.0 - 43.0 mil | Overall |
Arlon 940-07Bxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Thickness | 940 - 1090 microns | 37.0 - 43.0 mil | Overall |
Arlon 940-10Rxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Thickness | 889 - 1090 microns | 35.0 - 43.0 mil | Overall |
Arlon R34332X039 0.039" (0.991 mm) Fully Cured/Unsupported Design/Construction:Overall: Fully cured/unsupported This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.In.. |