Physical Properties Metric English Comments
Thickness 12.7 - 10000 microns
0.500 - 394 mil
Average value: 1440 microns Grade Count:15
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max..
Thickness 4000 - 10000 microns
157 - 394 mil
Microtherm Group Marineguard® Filament Reinforced Silica Marine Insulation Panel, Flexible and Waterproof
Microtherm Marineguard® is a lightweight flexible overstitched panel of high performance thermal insulation designed to form easily around complex shapes for optimized protection. The panels are ..
Thickness 9500 - 10000 microns
374 - 394 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (7 mm Molded Thickness)
AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 9500 - 10000 microns
374 - 394 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (9 mm Molded Thickness)
AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 8000 - 10000 microns
315 - 394 mil
Beijing Evergrow Resources BF-10 Basalt Needle Felt
Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi..
Thickness 9500 - 10000 microns
374 - 394 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 9500 - 10000 microns
374 - 394 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 9500 - 10000 microns
374 - 394 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness)
AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Thickness 9500 - 10000 microns
374 - 394 mil
Typical free lofted thickness after heating
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness)
AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..