Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 749 - 876 microns | 29.5 - 34.5 mil | Overall |
Arlon 55978X030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Cured/Uncured Layers Appearance: Gray silicone gum on glass fiber fabricThis data Represents typical values for the production material.. |
|||
Thickness | 749 - 876 microns | 29.5 - 34.5 mil | Overall |
Arlon 55578XA030M 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 749 - 876 microns | 29.5 - 34.5 mil | Overall |
Arlon R33468A030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured LayersAppearance: Semi-cured blue silicone gum on glass fabricThis data Represents typical values for the production material. .. |
|||
Thickness | 749 - 876 microns | 29.5 - 34.5 mil | Overall |
Arlon R34688XA030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured/Cured LayersThis data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |