Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon 920-05Bxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: ½” RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not requi.. |
|||
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon 920-07Rxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon 920-20Bxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon 920-20Txx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon LW201Xxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon LW202Bxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon LW202Txx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 533 - 584 microns | 21.0 - 23.0 mil | |
3M Panagraphics™ III Wide Width Flexible Substrate 22 mil white-pigmented vinyl substrate with a polyester scrim; Smooth front surface with a semi-gloss finish; Decorate first or second surface with inkjet direct printing or first surface with cut f.. |
|||
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon 920-15Rxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 1.5Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape.. |