Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 518581R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 920-20Txx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape
(discontinued **) Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 10842S020 0.020" (0.508 mm) Fully Cured, Unsupported, Silicone Rubber Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Side 1 |
Arlon 15370T020 0.020" (0.508 mm) Uncatalyzed, Unsupported Rubber on a Mylar Carrier Design/Construction:Side 1: Uncatalyzed, Unsupported Rubber on a Mylar CarrierAppearance: Translucent high viscosity gumThis data represents typical values for the production material. The data shou.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 30570R020 0.020" (0.508 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Side 1 |
Arlon 30570R020 0.020" (0.508 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 51583R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 57226R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 920-20Bxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon LW201Xxx-M1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Mylar Interleave Design/Construction:Cross Section Type: TriangularArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for subsequent.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon LW201Xxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon LW202Bxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon LW202Txx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon R32089R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon R35061R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon R35066R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 30580R020 0.020" (0.508 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 51268R020P 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Silicone RubberThickness:Side 1: Skim CoatSide 2: Skim Coat + 0.010" uncuredThis data Represents typical values for the product.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 51344R020 0.020" (0.508 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-Cured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 51420R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 51971R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data .. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 920-15Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 1.5Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon R33216R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon R33889R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information .. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon R34880T020 0.020" (0.508 mm) Uncatalyzed, Unsupported rubber on a Mylar Carrier Design/Construction:Side 1: Uncatalyzed, Unsupported rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 44602M020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberAppearance Tan rubber on glass fiber fabricThis data represents typical values for the production material. The data should not be used to write, or .. |