Physical Properties Metric English Comments
Thickness 241 - 292 microns
9.50 - 11.5 mil
Overall
Arlon 49581R101 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate  (discontinued **)&l
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The..
Thickness 241 - 292 microns
9.50 - 11.5 mil
Overall
Arlon 49581B010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
Thickness 241 - 292 microns
9.50 - 11.5 mil
Overall
Arlon 49581X010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place o..
Thickness 241 - 292 microns
9.50 - 11.5 mil
Overall
Arlon 49583R010 0.0105" (0.267 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, m..
Thickness 241 - 292 microns
9.50 - 11.5 mil
Overall
Arlon 49581XC010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Gray gum on glass fiber fabricThis data Represents typical values for the production material. The data ..
Thickness 191 - 292 microns
7.50 - 11.5 mil
Overall
Arlon R32521R010 0.0095" (0.241 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
Thickness 254 - 292 microns
10.0 - 11.5 mil
Side 2, Skim Coat + Uncured
Arlon R33216R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl..
Copyright © lookpolymers.com All Rights Reserved