Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 8.00 - 50.0 microns | 0.315 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex CL 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 106 are characterized by h.. |
|||
Thickness | 8.00 - 50.0 microns | 0.315 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® CL 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex CL 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 508 exhibit a good bal.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FG 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FG 106 are characterized by .. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FG 306 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 306 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, antiblocking and processing aid, suitable for blown film extrusion.Films manufactured with Clearf.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FG B3 Very Low Density Polyethylene Clearflex FG B3 is a linear low density polyethylene, with antioxidants, slip and antiblocking agents, suitable for blown film technology. The product is characterized by a very low density and a h.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FH 50 Linear Medium Density Polyethylene Clearflex FH 50 is a linear medium density polyethylene, with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FH 50 are characterized by a good balance between toug.. |
|||
Thickness | 8.00 - 50.0 microns | 0.315 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® H&T CLH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T CLH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CLH 108 show e.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene Clearflex H&T FGH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T FGH .. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Eraclene® FA 706 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 706 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Films manufactured with Eraclene FA 706 show good processability t.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Eraclene® FB 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FB 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Eraclene® FC 82 High Density Polyethylene - Blown Film Extrusion Eraclene FC 82 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully co.. |
|||
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene Flexirene FF 25 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FF 25 is characterized by a high elongational viscosi.. |
|||
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FG 20 F Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 F is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 F is recommended for the .. |
|||
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FG 20 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 U is recommended for the .. |
|||
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FG 23 I Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 I represents the version of Flexirene FG 20 I.. |
|||
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 are characterized by an.. |
|||
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 U are characterized b.. |
|||
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte.. |
|||
Thickness | 18.0 - 50.0 microns | 0.709 - 1.97 mil | Recommended |
Polimeri Europa Riblene® FM 50 Low Density Polyethylene - Blown Film Extrusion Riblene FM 50 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FM 50 is characterized by optimum optical properties and rigidity.Films manufactured with Riblene FM 50.. |
|||
Thickness | 30.0 - 50.0 microns | 1.18 - 1.97 mil | |
Premix Thermoplastics PRE-ELEC® ESD 4400 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 4400 is a static dissipative thermoplastic compound based on PE-LD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 4400 has been developed for .. |
|||
Thickness | 8.00 - 50.0 microns | 0.315 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CM 406 are characterized by h.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FF 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex FF 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FF 50.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® FG B0 Very Low Density Polyethylene Clearflex FG B0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FG B0 are highly transparent, have good sealing properties, even.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexire.. |
|||
Thickness | 18.0 - 50.0 microns | 0.709 - 1.97 mil | Recommended |
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe.. |
|||
Thickness | 5.00 - 50.0 microns | 0.197 - 1.97 mil | |
Möller Medical NanoSkin 90 NanoCoating Boiling-water resistant, non-abrasive, dirt-repellant, biocompatible coating with very good chemical resistance.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 25.0 - 50.0 microns | 0.984 - 1.97 mil | |
Möller Medical TafSkin 115 NanoCoating Non-abrasive PTFE coating with very good chemical resistance, and outstanding easy-to-clean properties, bioinert Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Clearflex® H&T LGH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LGH.. |
|||
Thickness | 10.0 - 50.0 microns | 0.394 - 1.97 mil | Recommended |
Polimeri Europa Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |