Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 221 microns | 8.70 mil | |
Hexcel® HexForce™ 348 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Thickness | 221 microns | 8.70 mil | |
Hexcel® HexForce™ 4450 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 221 microns | 8.70 mil | |
Hexcel® HexForce™ GA030 Carbon Fabric Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper.. |