Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 200 - 1200 microns | 7.87 - 47.2 mil | |
OCTAL DPET™ PET Sheet Clear rigid sheet for use in general packaging; foam, fill, and seal; dairy products; and lamination. DPET™ sheet is produced directly from PET melt resin, resulting in enhanced optical and mechan.. |
|||
Thickness | >= 200 microns | >= 7.87 mil | Minimum Web |
GrafTech GRAFCELL® FFP-200 SERIES Flow Field Plate Graphite Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid.. |
|||
Thickness | 200 - 3000 microns | 7.87 - 118.1 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.6 |
Sinotek Materials B Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Thickness | 200 microns | 7.87 mil | |
Shandong Dongyue Shenzhou New Material Co CHFM 200 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM) Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th.. |
|||
Thickness | 200 - 400 microns | 7.87 - 15.7 mil | |
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate) Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua.. |
|||
Thickness | 200 - 240 microns | 7.87 - 9.45 mil | |
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Thickness | 200 - 240 microns | 7.87 - 9.45 mil | |
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Thickness | 200 - 3000 microns | 7.87 - 118.1 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.5 |
Sinotek Materials A Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Thickness | 200 - 3000 microns | 7.87 - 118.1 mil | <1±0.03 :: 1-1.5±0.05 :: >1.5±0.7 |
Sinotek Materials C Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Thickness | 200 - 1200 microns | 7.87 - 47.2 mil | Average value: 404 microns Grade Count:8 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |