Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 178 microns | 7.00 mil | Backing |
Dielectric Polymers NT-5900HL Hot Air Leveling Tape
(discontinued **) Crosslinked silicone adhesive with polyester film and crepe paper backing.Features: High temperature resistantNo adhesive residue even when there is a delay between wave soldering and tape removalGo.. |
|||
Thickness | 178 - 1520 microns | 7.00 - 60.0 mil | |
Alcoa KAMA AgriHIPS 3500 AgriHIPS
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat.. |
|||
Thickness | 178 microns | 7.00 mil | HDPE Carrier |
Arlon 31580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on an HDPE Carrier
(discontinued * Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat.. |
|||
Thickness | 178 microns | 7.00 mil | Nominal |
DuPont™ Nomex® 419 Paper, 7 mil Nominal Thickness Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: .. |
|||
Thickness | 178 microns | 7.00 mil | silicone, side 2; Arlon SQA-TMS-003 |
Arlon 19646B025 Silicone Rubber/Fiberglass Laminate Side 1:cured silicone rubber; Substrate: 1523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7046 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7046 and 7053 are durable, high performance materials that offer excellent durability and moisture resistance. These vinyl label stocks utilize.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7049 Screen Printable Extended Life Vinyl Performance Label Products 3M™ Screen Printable Extended Life Vinyl Performance Label Products are high performance materials that offer good conformability and moisture resistance. These vinyl label stocks utilize 3M™ Adhe.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7051 Screen Printable Extended Life Vinyl Performance Label Products 3M™ Screen Printable Extended Life Vinyl Performance Label Products are high performance materials that offer good conformability and moisture resistance. These vinyl label stocks utilize 3M™ Adhe.. |
|||
Thickness | 178 microns | 7.00 mil | Carrier; Arlon SQA-TMS-003 |
Arlon 31940C025 0.025" (0.635 mm) Uncured Silicone Rubber on HDPE Carrier Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberCarrier: HDPEThis data represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 178 microns | 7.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
Thickness | 178 microns | 7.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 56596R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Thickness | 178 - 330 microns | 7.00 - 13.0 mil | Overall |
Arlon 910-05RXX-P0 0.010" (0.254 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Thickness | 178 - 229 microns | 7.00 - 9.00 mil | Side 1 |
Arlon R34172W008 0.008" (0.203 mm) Cured, Unsupported Silicone Rubber on a Mylar Carrier Design/Construction:Side 1: Cured, Unsupported Silicone Rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FM165 Indoor UL Recognized Computer Imprintable White Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable White Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FV095 Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Thickness | 178 microns | 7.00 mil | |
3M Scotch® 2510 Varnished Cambric Tape Scotch® Varnished Cambric Tapes are made from straight-cut woven cotton cambric fabric. The fabric is oil primed and coated with a high-grade yellow electrical insulating varnish. Varnished cambric.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-10 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-85 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ IJ680-10 Reflective Graphic Film 6-mil flexible, enclosed lens, retroreflective films; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Pressure.. |
|||
Thickness | 178 microns | 7.00 mil | Total; ASTM D3752 |
3M 398FRP Printed Version Glass Cloth Tape 3M™ Glass Cloth Tape 398FRP has an acrylic adhesive for many applications requiring high adhesion, an abrasion-resistant backing and flame retardant properties. This product is typically used for s.. |
|||
Thickness | 178 microns | 7.00 mil | Total without liner; ASTM D3752 |
3M 5430 Squeak Reduction Tape 3M™ Squeak Reduction Tapes are a film tape for the automotive industry to help control squeaks and rattles due to vibration or wear of metal and plastic materials.Information provided by 3M |
|||
Thickness | 178 microns | 7.00 mil | Overall; Arlon SQA-TMS-003 |
Arlon 47571R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PESide 1: Uncured Silicone Rubber Substrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Appearance: Red silicone gum on fibergl.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7034 Screen Printable Polyester Performance Label Products 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7053 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7046 and 7053 are durable, high performance materials that offer excellent durability and moisture resistance. These vinyl label stocks utilize.. |
|||
Thickness | 178 microns | 7.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55103R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber This data represents typical values for the production materia.. |
|||
Thickness | 178 microns | 7.00 mil | Polyester |
3M 7961MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Thickness | 178 microns | 7.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55149R028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FM055 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Thickness | 178 microns | 7.00 mil | layer 2; Arlon SQA-TMS-003 |
Arlon 55279R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass |