Physical Properties Metric English Comments
Thickness 1680 microns
66.1 mil
Standard; Laminate
GrafTech GRAFOIL® GHJ Non-Standard Internal Combustion Grade GHJ Laminate, Metal Reinforced
GRAFOIL® Grade GHJ is a laminate made with GRAFOIL® Grade GTC flexible graphite mechanically attached to a perforated, low-carbon steel core. Its applications include: exhaust manifold gasket..