Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1630 microns | 64.2 mil | Standard; Laminate |
GrafTech GRAFOIL® GHE Standard Fluid Sealing Laminate, Metal Reinforced GRAFOIL® Grade GHE laminate is made with GTB flexible graphite mechanically bonded to both faces of a 316 or 316L stainless steel tang metal insert. Surface identifiable, the laminate is branded .. |
|||
Thickness | 1630 microns | 64.2 mil | Standard; Laminate |
GrafTech GRAFOIL® GHH Standard Internal Combustion Laminate, Metal Reinforced GRAFOIL® Grade GHH is a laminate made with GRAFOIL® Grade GTC flexible graphite chemically bonded to both faces of a flat, low-carbon steel core. Its applications include: exhaust sealing, ga.. |