Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 155 microns | 6.10 mil | |
Hexcel® HexForce™ 1680 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 155 microns | 6.10 mil | Liner |
3M 470 Electroplating Tape 3M™ Electroplating Tape 470 is a conformable and abrasion-resistant vinyl tape with excellent resistance to most chemicals used in typical electroplating processes.Information provided by 3M |
|||
Thickness | 155 microns | 6.10 mil | Liner |
3M 470L Electroplating Tape 3M™ Electroplating Tape 470L is a linered version of 3M vinyl tape 470 that may be used for die-cutting or large area applications.Information provided by 3M |
|||
Thickness | 155 microns | 6.10 mil | ASTM D3652 |
3M ARMR220 NC Anti-Reflection Matte Removable Non-Conductive Protection Film 3M™ ARMR220 NC Protection Film uses 3M’s advanced coating technology to provide durable protection, reflection reduction for a clear image, with a residue-free, self-wetting adhesive for applicati.. |
|||
Thickness | 155 microns | 6.10 mil | Tab; ASTM D3652 |
3M ScotchPad™ 818CP Custom Printed Marking Tapes 3M™ ScotchPad™ Custom Printed Marking Taps 818CP are individual paper tags laminated to the strongest conformable backing and most consistent pressure-sensitive hot-melt adhesive system available... |
|||
Thickness | 155 microns | 6.10 mil | ASTM D3652 |
3M GLS100 Glossy Protection Film 3M™ Glossy Protection Film uses 3M’s coating technology to provide durable protection with a residue-free, self-wetting adhesive for application on electronic displays.Information provided by 3M |