Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1470 - 1570 microns | 58.0 - 62.0 mil | Overall |
Arlon LW601Xxx-P1 0.060" (1.52 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction: Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for su.. |
|||
Thickness | 1470 - 1730 microns | 58.0 - 68.0 mil | Overall |
Arlon R35121R063 0.063" (1.60 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material speci.. |
|||
Thickness | 1470 - 1730 microns | 58.0 - 68.0 mil | Overall |
Arlon R31246R063 0.063" (1.60 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate.. |
|||
Thickness | 1470 - 1730 microns | 58.0 - 68.0 mil | Overall |
Arlon R34256R063 0.063" ((1.60 mm) Uncured/Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate.. |