Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 147 microns | 5.80 mil | |
Hexcel® HexForce™ 6557 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 147 microns | 5.80 mil | Total; ASTM D3752 |
3M 363LC High Temperature Aluminum Foil/Glass Cloth Tape 3M™ High Temperature Aluminum Foil/Glass Cloth Tape 363LC can be used as a high temperature, heat reflective, protective wrap for certain cables and other components in aerospace and industrial app.. |
|||
Thickness | 147 microns | 5.80 mil | Prepreg thickness - glass style 2112 |
Arlon 25FR Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
Thickness | 147 microns | 5.80 mil | Prepreg thickness - glass style 2112 |
Arlon 25N Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
Thickness | 147 microns | 5.80 mil | Tape |
3M 9425 Repositionable Tape 3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M |
|||
Thickness | 147 microns | 5.80 mil | Liner |
3M FM118B Indoor UL Recognized MC Polyester Label Products 3M™ Indoor UL Recognized MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These po.. |
|||
Thickness | 147 microns | 5.80 mil | Liner |
3M FM12B Indoor UL Recognized White Polyester Label Products 3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A.. |
|||
Thickness | 147 microns | 5.80 mil | Liner |
3M FM14B Indoor UL Recognized Computer Imprintable Clear Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Thickness | 147 microns | 5.80 mil | Liner |
3M FM15B Indoor UL Recognized Computer Imprintable Silver Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products a.. |
|||
Thickness | 147 microns | 5.80 mil | Liner |
3M FV06B Semi-Rigid White Vinyl Label Product 3M™ Semi-Rigid White Vinyl Label Products are white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clarity general.. |
|||
Thickness | 147 microns | 5.80 mil | Liner |
3M FV09B Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Thickness | 147 microns | 5.80 mil | without adhesive |
3M Scotchcal™ IJ66 Perforated Window Graphic Film Film IJ66 is a 5.8-mil vinyl with a 40% perforated pattern and a removable, pressure-sensitive adhesive. This film allows a full image to be seen on the outside of a window while allowing viewing th.. |
|||
Thickness | 147 microns | 5.80 mil | Liner |
3M FM16B Indoor UL Recognized Computer Imprintable White Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable White Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Thickness | 147 microns | 5.80 mil | ASTM D3652 |
3M 1900 Specialty High Temperature Masking Tape 3M™ Value Duct Tape 1900 is a conformable cloth duct tape made with polyethylene film over cloth scrim and rubber adhesive. A good choice for non-critical applicationsInformation provided by 3M |
|||
Thickness | 147 microns | 5.80 mil | Backing; ASTM D3752 |
3M 5153 PTFE Glass Cloth Tape 3M™ PTFE Glass Cloth Tape 5151 is constructed using (PTFE) polytetra-fluoroethylene impregnated glass cloth and silicone adhesive. This tape is used in many applications requiring high temperature .. |