Thickness 145 microns
5.70 mil
Hexcel® HexForce™ 1064 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 145 microns
5.70 mil
ASTM D3652
3M Scotch® 8959 Bi-Directional Filament Tape
Scotch® Filament Tape 8959 is a bi-directional specialty packaging tape reinforced with continuous glass yarns in both the longitudinal and transverse direction along with a biaxially oriented poly..
Thickness 145 microns
5.70 mil
3M Scotch Pad™ 819 Filament Tape Pads
3M™ ScotchPad™ Filament Tape Pad 819 is a pre-cut pad formed with layered high performance filament tape sheets featuring biaxially oriented polypropylene backing with continuous glass yarns that ..