Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 140 microns | 5.50 mil | Liner |
Dielectric Polymers NT-100A89 General Purpose Laminating Adhesive
(discontinued **) Acrylic adhesive with moisture stable PE coated kraft (89#) liner.Features: Plasticizer migration resistantChemical resistantMoisture resistantApplications: Mounting nameplates, signs, graphic panel.. |
|||
Thickness | 140 microns | 5.50 mil | Liner |
Dielectric Polymers NT-140A89 General Purpose Laminating Adhesive
(discontinued **) Acrylic adhesive with moisture stable PE coated kraft (89#) liner.Features: Plasticizer migration resistantChemical resistantMoisture resistantApplications: Mounting nameplates, signs, graphic panel.. |
|||
Thickness | 140 microns | 5.50 mil | |
Hexcel® HexForce™ 1557 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 140 microns | 5.50 mil | Typical; TAPPI-411 |
DuPont™ Nomex® 411 Paper, 5 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Thickness | 140 - 216 microns | 5.50 - 8.50 mil | Side 2 |
Arlon 19576R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat.. |
|||
Thickness | 140 microns | 5.50 mil | Style 1681 Fiberglass, Substrate; Arlon SQA-TMS-003 |
Arlon 49481R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Thickness | 140 microns | 5.50 mil | Prime Coated 1681 Fiberglass, Substrate |
Arlon 49576R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat.. |
|||
Thickness | 140 microns | 5.50 mil | Prime Coated 1681 Fiberglass, Substrate |
Arlon 49581R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The.. |
|||
Thickness | 140 microns | 5.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51866R015 0.0170" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 140 microns | 5.50 mil | Substrate; Arlon SQA-TMS-003 |
Arlon R38026B017 0.017" (0.432 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured Silicone Rubber Interleave: LDPEThis data represents typical values for the production material. The.. |
|||
Thickness | 140 microns | 5.50 mil | ASTM D3652 |
3M Scotch® 892 Filament Tape Scotch® Tape 892 is a glass filament reinforced tape suitable for most strapping, bundling, and reinforcing applications. The tape has a synthetic rubber resin adhesive with good shear strength to .. |
|||
Thickness | 140 microns | 5.50 mil | Backing; ASTM D3652 |
3M 434/Silver Damping Foils Low temperature vibration dampingInformation provided by 3M |
|||
Thickness | 140 microns | 5.50 mil | Prime Coated 1165 Fiberglass, Substrate |
Arlon 44571R008A 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 140 microns | 5.50 mil | substrate; Arlon SQA-TMS-003 |
Arlon 49283R040 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil polyethylene; Side 1: cured silicone rubber; Substrate: 1681 Fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 140 microns | 5.50 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 49586B010 0.0115" (0.292 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater.. |
|||
Thickness | 140 microns | 5.50 mil | side 2 silicone; Arlon SQA-TMS-003 |
Arlon 51146R015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 140 microns | 5.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51576W015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: White silicone gum on glass fabricThis data re.. |
|||
Thickness | 140 - 216 microns | 5.50 - 8.50 mil | Side 1 |
Arlon 51970R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, or .. |
|||
Thickness | 140 microns | 5.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51986XA015 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Gray silicone gum and rubber on fiberglass clo.. |
|||
Thickness | 140 microns | 5.50 mil | Prime Coated 1165 Fiberglass, Substrate |
Arlon R33826R017 0.017" (0.432mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 140 - 165 microns | 5.50 - 6.50 mil | Film and adhesive |
3M 3635-100 Light Enhancement Film A light box or channel letter contains lighting elements that illuminate the front sign face and transmit some light to the viewer. However much of the illumination is reflected or absorbed by other.. |
|||
Thickness | 140 microns | 5.50 mil | Tape Only |
3M 469 Splicing Tape 3M™ Splicing Tapes utilize an acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Thickness | 140 microns | 5.50 mil | Total Thickness |
3M 9731 Double Coated Tape 3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other .. |
|||
Thickness | 140 microns | 5.50 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 44562R011 0.011" Cured Silicone Rubber with Fiberglass Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Thickness | >= 140 microns | >= 5.50 mil | Side 2 |
Arlon 44686W013 0.013" (0.330 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber UL Recognition: 220°C per UL Card E54153Appearance: White silicone gum on fiberglassThis data represents typical val.. |
|||
Thickness | 140 microns | 5.50 mil | Overall; Arlon SQA-TMS-003 |
Arlon 440-638RF 0.0055" (0.140 mm) Style 1165 Plain Weave, Prime Coated Fiberglass Design/Construction:Fiberglass Fabric primed for adhesion to silicone elastomers vulcanized with organic peroxides.Material: Prime Coated FiberglassCount: 60x52 (Ends x Picks)This data represents ty.. |
|||
Thickness | 140 microns | 5.50 mil | Overall Thickness |
Arlon 48576R006 0.0055" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.0015" PolyethyleneSide 1: Uncured RubberSubstrate: Prime Coated 1080 FiberglassSide 2: Uncured RubberThis data represents typical values for the production mater.. |
|||
Thickness | 140 microns | 5.50 mil | Overall thickness; Arlon SQA-TMS-003 |
Arlon R37582R0055 0.0055" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Thickness | 140 microns | 5.50 mil | Overall thickness; Arlon SQA-TMS-003 |
Arlon R3758R0055 0.065" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Thickness | 140 microns | 5.50 mil | Overall; Arlon SQA-TMS-003 |
Arlon R37652R0055 0.0055" (0.140 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 2113 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. .. |