Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 127 - 2540 microns | 5.00 - 100 mil | Range of Standard Thicknesses |
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowTight dielectric constant and thickness control for repeatable circuit performanceLow moi.. |
|||
Thickness | 127 - 2540 microns | 5.00 - 100 mil | Range of Standard Thicknesses |
Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowLow Z-axis expansion. Provides reliable plated through holes in multi-layer boardsTight .. |
|||
Thickness | 127 microns | 5.00 mil | |
GrafTech eGRAF® HITHERM™ HT-1205 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Thickness | 127 microns | 5.00 mil | ASTM D3652 |
3M 4195-EZ Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 4195-EZ is an easy unwind tapes coated with a very high-tack adhesive system to help provide temporary protection of automotive carpets, fabric interiors and carpe.. |
|||
Thickness | 127 microns | 5.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 22122R079 0.079" Cured Silicone Rubber and FEP Film Laminate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: 0.005" FEP FilmThis data represents typical values for the production material and should not be used as .. |
|||
Thickness | 127 microns | 5.00 mil | Mylar on Side 2 |
Arlon 28561R015M 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. T.. |
|||
Thickness | 127 microns | 5.00 mil | ASTM D3752 |
3M 764 General Purpose Vinyl Tape 3M™ General Purpose Vinyl Tape 764 can be used in non-critical applications such as color coding, bundling and safety marking, etc.Information provided by 3M |
|||
Thickness | 127 microns | 5.00 mil | Carrier; Arlon SQA-TMS-003 |
Arlon 32580R035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. .. |
|||
Thickness | >= 127 microns | >= 5.00 mil | Side 2 |
Arlon 49576R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat.. |
|||
Thickness | 127 microns | 5.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55572AA024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be us.. |
|||
Thickness | 127 microns | 5.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon R30711R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: PolyethyleneAppearance: Red silicone gum .. |
|||
Thickness | 127 microns | 5.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon R30711R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: PolyethyleneAppearance: Red silicone gum .. |
|||
Thickness | 127 microns | 5.00 mil | Substrate |
Arlon R32390B020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1165 FiberglassAll ingredients of product are listed in 21 CFR 177.26000This data represe.. |
|||
Thickness | 127 microns | 5.00 mil | Tape |
3M XT2112 Hi-Tack Adhesive Transfer Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range o.. |
|||
Thickness | 127 microns | 5.00 mil | Tape |
3M XT2112-AGT Hi-Tack Adhesive Transfer Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product constructions to support demanding application requirements. This product line provides a range o.. |
|||
Thickness | 127 microns | 5.00 mil | Layer 2; Arlon SQA-TMS-003 |
Arlon 51149R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberSubstrate: Style 7628 FiberglassLayer 1: Cured Silicone RubberThis data represents typical values for the production mat.. |
|||
Thickness | 127 - 152 microns | 5.00 - 6.00 mil | Side 2 |
Arlon 51971R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data .. |
|||
Thickness | 127 microns | 5.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55271R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Interleave 2: Polyethylene Product Use: Flexible heater in.. |
|||
Thickness | 127 microns | 5.00 mil | Side 1 |
Arlon 56096R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 127 microns | 5.00 mil | Tape Only |
3M 950 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer adhesion to a wide variety of surfaces, including many plastics. This pressure-sensitive medium firm acrylic adhesive family features a very.. |
|||
Thickness | 127 microns | 5.00 mil | Liner |
3M OFM1605 Outdoor UL Recognized Clear Polyester Label Product 3M™ Outdoor UL Recognized Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Thickness | 127 microns | 5.00 mil | ASTM D3652 |
3M 51825 Industrial Polyethylene Temporary Surface Protection Tape 3M™ Industrial Polyethylene Temporary Surface Protection Tape51825 is a very low adhesion temporary protection tape designed for a variety of surface protection applications.Information provided by.. |
|||
Thickness | 127 microns | 5.00 mil | Substrate |
Arlon 41580R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Thickness | 127 microns | 5.00 mil | Prime Coated 1165 Fiberglass, Substrate |
Arlon 44560R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w.. |
|||
Thickness | 127 microns | 5.00 mil | Prime Coated 1165 Fiberglass, Substrate |
Arlon 44570R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Layers Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be use.. |
|||
Thickness | 127 microns | 5.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 44981R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene UL Recognition File: E54153.. |
|||
Thickness | 127 microns | 5.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 44981R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene UL Recognition File: E54153.. |
|||
Thickness | 127 microns | 5.00 mil | Substrate |
Arlon R37732R079 0.079" (2.01 mm) Cured Silicone Rubber with FEP Film Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: FEP FilmAppearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical value.. |
|||
Thickness | 127 microns | 5.00 mil | Carrier |
Arlon 32400N030 0.030" (0.762 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PET Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for the productio.. |
|||
Thickness | 127 microns | 5.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 44278R018 0.018" Uncured/Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate Design/Construction:Interleave 1: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEUL.. |