Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 124 microns | 4.87 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP3015-WH High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. White-ceramic inorganic coating to 1500°F. |