Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 112 microns | 4.40 mil | Total |
Parker Chomerics CHO-FOIL CCD Shielding Tape Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti.. |
|||
Thickness | 112 microns | 4.40 mil | ASTM D3652 |
3M 201+ General Use Masking Tape 3M™ General Use Masking Tape 201+ is a tan colored crepe paper masking tape for holding, bundling, sealing, non-critical masking applications and a vast number of other jobs where a pressure sensit.. |
|||
Thickness | 112 microns | 4.40 mil | Total; ASTM D3652 |
3M 3367 General Purpose Aluminum Foil Tape 66 lb moisture stable liner. Good for die-cut applications.Information provided by 3M |
|||
Thickness | 112 microns | 4.40 mil | Caliper |
3M 9496LE High Strength Double Coated Tape with Adhesives 300LSE and 200MP 3M™ Double Coated Tape 9496LE with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and.. |
|||
Thickness | 112 microns | 4.40 mil | ASTM D3652 |
3M 200 Paper Tape 3M™ Paper Tape 200 is a utility purpose paper tape for holding, bundling, sealing, non-critical masking and a vast number of other jobs where a pressure-sensitive tape is needed.Information provide.. |