Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 940 microns | 37.0 mil | |
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
Thickness | 940 microns | 37.0 mil | Standard |
GrafTech eGRAF® SPREADERSHIELD™ SS300 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Thickness | 940 microns | 37.0 mil | Standard |
GrafTech eGRAF® SPREADERSHIELD™ SS400 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Thickness | 940 microns | 37.0 mil | Standard; Laminate |
GrafTech GRAFOIL® TG-251 Standard Internal Combustion Laminate, Metal Reinforced GRAFOIL® Grade TG-251 is GRAFOIL® Grade GTC flexible graphite chemically bonded to both faces of a flat, low-carbon steel core. Its applications include: exhaust sealing, gasoline/diesel head.. |
|||
Thickness | 940 microns | 37.0 mil | Total; ASTM D3752 |
3M 1532 Sandblast Stencil 3M™ Sandblast Stencil 1532 is a tan rubber sandblast stencil featuring a polyester liner for use in a variety of sandblasting protection applications, including pavers, stone and glass surfaces.Inf.. |
|||
Thickness | 940 microns | 37.0 mil | Total; ASTM D3752 |
3M 1532S Sandblast Stencil 3M™ Sandblast Stencil 1532S is a tan rubber sandblast stencil featuring a polyester liner for use in a variety of sandblasting protection applications, including pavers, stone and glass surfaces.In.. |
|||
Thickness | 940 microns | 37.0 mil | Total; ASTM D3752 |
3M 1532T Sandblast Stencil 3M™ Sandblast Stencil 1532T is a tan rubber sandblast stencil featuring a polyester liner for use in a variety of sandblasting protection applications, including pavers, stone and glass surfaces.In.. |
|||
Thickness | 940 - 1090 microns | 37.0 - 43.0 mil | Overall |
Arlon 25122R040 0.040" (1.02 mm) Silicone Rubber on Laminated Fluoropolymer Film Appearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical values for the production material. The data should not be used to write, or in place of, material.. |
|||
Thickness | 940 - 1090 microns | 37.0 - 43.0 mil | Overall |
Arlon 940-07Rxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Thickness | 940 - 1090 microns | 37.0 - 43.0 mil | Overall |
Arlon 940-07Rxx-P1 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Performance Advantages:Resists moisture, oxygen, and ozone to assure continuous high insulation values.Conforms smoothly when wr.. |
|||
Thickness | 940 microns | 37.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R39118R037L 0.037" (0.940 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyester Release Liner Transfer Pressure Sensitive Adhesive: Silicone PSASide 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Cured Silicone Rubber.. |
|||
Thickness | 940 microns | 37.0 mil | with liner |
3M GM400 Gripping Material 3M™ Gripping Material GM400 is based on 3M’s proprietary micro-replicated technology. 3M™ Gripping Material GM110 is based on 3M’s proprietary micro-replicated technology. 3M griping material GM.. |
|||
Thickness | 940 microns | 37.0 mil | |
3M Nextel™ CF-40 Woven Fabric 550 Information provided by 3M |
|||
Thickness | 940 microns | 37.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 51271R037 0.037" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ.. |
|||
Thickness | 940 - 1090 microns | 37.0 - 43.0 mil | Overall |
Arlon 940-07Bxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Thickness | 940 - 1090 microns | 37.0 - 43.0 mil | Overall |
Arlon 940-10Rxx-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Thickness | 940 microns | 37.0 mil | |
3M Nextel™ AF-40 Industrial Woven Fabric 312 Information provided by 3M |