Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 78.7 microns | 3.10 mil | Total; ASTM D3652 |
3M 1450 General Purpose Aluminum Foil Tape High tack adhesive for good, instant adhesion to many surfaces.Information provided by 3M |
|||
Thickness | 78.7 microns | 3.10 mil | Liner Caliper |
3M 9088FL High Performance Double Coated Tapes with Adhesive 375 3M™ Double Coated Tapes with 3M™ Adhesive 375 provides a high level of adhesive peel and shear performance. The adhesive system used on these products provides good adhesion to both high and low s.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FA112 Destructible Acetate Label Products 3M™ Destructible Acetate Label Products FA102 and FA112 offer consistent, high quality film that fractures when attempting label removal from many surfaces. These acetate labels utilize 3M™ Adhesi.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FM022 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FM042 Clear Polyester Label Product 3M™ Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for demanding applications such.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FM052 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FM058 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FM06E Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FM092 Indoor UL Recognized Matte Silver Polyester Label Product 3M™ Indoor UL Recognized Matte Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FM122R Indoor UL Recognized White Polyester Label Products 3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FM1542 Clear Polyester Label Products 3M™ Clear Polyester Label Products FM1541 and FM1542 are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesi.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FM298 Indoor UL Recognized Clear Polyester Overlaminate Label Products 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FM53R2 White Polyester Label Products 3M™ White Polyester Label Products FM53R2, FM532 and FM782 are durable, high performance materials that utilize 3M™ Adhesive P1110, which is for labeling tires when used with tire wash. This adhes.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FP012602 White Polyester Label Products ion 3M™ White Polypropylene Label Products are glossy white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FP085 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FP0868 Removable Clear Polypropylene Label Products 3M™ Removable Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ultra removable acrylic designed f.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FP08P Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FS022 Clear Polystyrene Label Products 3M™ Clear Polystyrene Label Products are hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive P1212, which is a high c.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FV052R Tire Vinyl Label Products 3M™ Tire Vinyl Label Products are white vinyl label stocks that offer durability and conformability. These vinyl labels utilize 3M™ Adhesive P1110, which is designed for labeling tires when used w.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FV092 Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FV092R Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FV1222 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are soft white vinyl label stocks that offer durability and good conformability. These vinyl labels utilize 3M™ Adhesive R3500, which is designed for use on smoo.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M OFL0208 Outdoor UL Recognized Lexan Label Products 3M™ Outdoor UL Recognized Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M OFM03402 Outdoor UL Recognized White Polyester Label Product 3M™ Outdoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FP022102 White Polypropylene Label Product 3M™ White Polypropylene Label Products FP022101, FP022102, FP022108, FP026002, FP02600N and FP026009 are matte white opaque materials that offer excellent durability and moisture resistance. These .. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FS502 White Polystyrene Label Products 3M™ White Polystyrene Label Products FS501, FS502 and FS532 are hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive R.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M FV1002 Soft White Vinyl EDP Label Product 3M™ Soft White Vinyl EDP Label Products FV100K and FV1002 are flexible vinyl label stocks that offer excellent durability and some moisture resistance. These vinyl labels utilize 3M™ Adhesive F220.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M PS102 Semi-gloss Paper Label Product 3M™ Semi-gloss Paper Label Product PS102 is a durable, general purpose paper product. This label product utilizes 3M™ Adhesive P1110, which is for labeling tires when used with tire wash. This adh.. |
|||
Thickness | 78.7 microns | 3.10 mil | Liner |
3M PS442 White Yupo™ EDP Label Product 3M™ White Yupo™ EDP Label Product PS442 is a matte white polypropylene material that offers excellent durability. This label product utilizes 3M™ Adhesive P1110, which is a general purpose perman.. |
|||
Thickness | 78.7 microns | 3.10 mil | recommended dry film thickness |
Aremco Corr-Paint™ CP2020 High Temperature Protective Coating Urethane, Aluminum Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |