Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 737 microns | 29.0 mil | nom |
Mid-Mountain Materials SILTEX® 18 Amorphous Silica Textile Description: SILTEX is a family of high performance textile fabric that is comprised of high purity, high strength amorphous silica fibers, woven into a strong, flexible fabric designed for use wher.. |
|||
Thickness | 737 microns | 29.0 mil | Nominal |
DuPont™ Nomex® 410 Paper, 29 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Thickness | 737 - 787 microns | 29.0 - 31.0 mil | Overall |
Arlon 55579R028M 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured layer on top of a cured layer on one side This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 737 - 813 microns | 29.0 - 32.0 mil | Overall |
Arlon 55609R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThi.. |
|||
Thickness | 737 microns | 29.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55759R028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass This data represents typical values for the production ma.. |
|||
Thickness | 737 microns | 29.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 56609R028 0.029" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production materi.. |
|||
Thickness | 737 - 889 microns | 29.0 - 35.0 mil | Side 1 |
Arlon 75400R045 0.045" (1.14 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Thickness | 737 - 787 microns | 29.0 - 31.0 mil | Overall |
Arlon R33089X028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 737 - 813 microns | 29.0 - 32.0 mil | Overall |
Arlon R33099G028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl.. |
|||
Thickness | 737 - 813 microns | 29.0 - 32.0 mil | Overall |
Arlon R34369R028 0.029" (0.737 mm) Uncured Layer on Top of a Cured Layer on One Side with Fiberglass Substrate, 38" wide Design/Construction:Side 1: Uncured Layer on Top of a Cured Layer on One SideThis data Represents typical values for the production material. The data should not be used to write, or in place of, ma.. |