Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 724 microns | 28.5 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55629R028 0.0285" (0.724 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglassThis data repre.. |
|||
Thickness | 724 microns | 28.5 mil | |
Hexcel® HexForce™ 690 Carbon Fabric Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper.. |