Physical Properties Metric English Comments
Thickness 640 microns
25.2 mil
Standard
GrafTech GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material
GRAFOIL® GTA premium flexible graphite is a non-inhibited grade developed for use in nuclear or semiconductor applications. It is certified to meet the most rigorous purity specifications of the ..
Thickness 640 microns
25.2 mil
Standard
GrafTech GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material
GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typicall..
Thickness 640 microns
25.2 mil
Standard
GrafTech GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material
GRAFOIL® GTC flexible graphite sheet is a gasketing material containing no binders or fillers, which will seal a wide variety of liquids and gases over an extremely large temperature range. GTC c..