Thickness 597 - 673 microns
23.5 - 26.5 mil
Overall
Arlon 19562R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wr..
Thickness 597 - 673 microns
23.5 - 26.5 mil
Overall
Arlon 19566R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The..
Thickness 597 - 673 microns
23.5 - 26.5 mil
Overall
Arlon 19576R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat..
Thickness 597 - 673 microns
23.5 - 26.5 mil
Overall
Arlon R34896R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of..