Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 510 - 5100 microns | 20.1 - 201 mil | ASTM D374 |
Parker Chomerics THERM-A-GAP™ G174 Cost Effective Gap Filler Description: THERM-A-GAP™ elastomers are used to fill air gaps between PC boards or other components and heat sinks, metal enclosures, and chassis. The exceptional conformability of these advanced .. |
|||
Thickness | 510 - 12700 microns | 20.1 - 500 mil | |
Parker Chomerics WIN-SHIELD™ A (Acrylic) EMI Shielded Window Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate, acrylic and cast polycarbonate. A unique feature of Parker Chomerics w.. |
|||
Thickness | 510 - 12700 microns | 20.1 - 500 mil | Plastic |
Parker Chomerics WIN-SHIELD™ ITO (Coated) EMI Shielded Window Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate, acrylic and cast allycarbonate. A unique feature of Parker Chomerics w.. |
|||
Thickness | 510 - 12700 microns | 20.1 - 500 mil | |
Parker Chomerics WIN-SHIELD™ P (Polycarbonate) EMI Shielded Window Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate, acrylic and cast polycarbonate. A unique feature of Parker Chomerics w.. |
|||
Thickness | 510 microns | 20.1 mil | Standard |
GrafTech eGRAF® SPREADERSHIELD™ SS300 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Thickness | 510 microns | 20.1 mil | Standard |
GrafTech eGRAF® SPREADERSHIELD™ SS400 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Thickness | 510 microns | 20.1 mil | Standard |
GrafTech GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material GRAFOIL® GTA premium flexible graphite is a non-inhibited grade developed for use in nuclear or semiconductor applications. It is certified to meet the most rigorous purity specifications of the .. |
|||
Thickness | 510 microns | 20.1 mil | Standard |
GrafTech GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typicall.. |
|||
Thickness | 510 microns | 20.1 mil | Standard |
GrafTech GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material GRAFOIL® GTC flexible graphite sheet is a gasketing material containing no binders or fillers, which will seal a wide variety of liquids and gases over an extremely large temperature range. GTC c.. |
|||
Thickness | 510 microns | 20.1 mil | Standard |
GrafTech GRAFOIL® GTX Standard Fluid Sealing Graphite, Single Layer Material GRAFOIL® GTX flexible graphite sheet is inhibited for high oxidation/corrosion resistance that can be used for most fluid sealing and industrial applications. Grade GTX contains an inorganic, non.. |
|||
Thickness | 510 microns | 20.1 mil | |
3M Nextel™ AF-20 Industrial Woven Fabric 312 Information provided by 3M |
|||
Thickness | 510 microns | 20.1 mil | |
3M Nextel™ BF-20 Woven Fabric 440 Information provided by 3M |