Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 67.1 microns | 2.64 mil | Wet Film |
Aremco Glass-Coat™ GC4000 High Temperature Specialty Coatings Glass Glass-enamel, gloss-black coating for stainless steel to 1000°F (538°C) |
|||
Thickness | 67.1 microns | 2.64 mil | Wet Film |
Aremco Glass-Coat™ SGC4000 High Temperature Specialty Coatings Silicone-Glass Silicone-glass-ceramic, gray, low viscosity, scratch resistant coating for stainless steel to 900°F (482°C) |