Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 60.0 microns | 2.36 mil | Average value: 60.0 microns Grade Count:4 |
Overview of materials for Ethylene Acrylic Acid This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Thickness | 60.0 microns | 2.36 mil | ± 3.0%; ASTM-252-78 |
Kinlead PT21 Adhesive Tape Grade BOPP Plain Film (thickness: 60 µm) PT21 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion. Both sides have corona treatment. It is widely used in industrial adh.. |
|||
Thickness | 60.0 microns | 2.36 mil | |
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Thickness | 60.0 microns | 2.36 mil | |
Dow Primacor® 1321 Ethylene Acrylic Acid (EAA) PRIMACOR® 1321 polymer is an EAA copolymer (% comonomer 6.5) for blown and cast films. Its outstanding properties include, excellent sealability, toughness, adhesion and tear resistance. PRIMACOR 1.. |
|||
Thickness | 60.0 microns | 2.36 mil | |
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Thickness | 60.0 microns | 2.36 mil | |
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Thickness | 60.0 microns | 2.36 mil | Total; Standards |
CEN® Electronic Material CS Polyimide Tape CEN® CS polyimide tape is made of CEN® CN polyimide film coated with a high performance silicone adhesive. The tape shows excellent dielectric and insulation properties, high heat resistant, excel.. |