Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 58.4 microns | 2.30 mil | |
Dow DOWLEX™ 2247G Polyethylene Resin Next Generation DOWLEX™ 2247G Polyethylene Resin with Extra Stretch Performance (ESP) is an ethylene-octene-1 copolymer designated for cast stretch film applications, such as industrial pallet wrap.. |
|||
Thickness | 58.4 microns | 2.30 mil | Faceside Adhesive |
3M 3028EK Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Thickness | 58.4 microns | 2.30 mil | Backside Adhesive |
3M 3028EK Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Thickness | 58.4 microns | 2.30 mil | |
3M 941 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Thickness | 58.4 microns | 2.30 mil | Faceside Adhesive |
3M 9500B Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Thickness | 58.4 microns | 2.30 mil | Faceside Adhesive |
3M 9500PC Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Thickness | 58.4 microns | 2.30 mil | |
3M 9502 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Thickness | 58.4 microns | 2.30 mil | |
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thickness | 58.4 microns | 2.30 mil | Total Thickness |
3M 9824 Double Coated Tapes with Adhesive 340 3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP012202 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP0122R2 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP012615 White Polyester Label Products ion 3M™ White Polypropylene Label Products are glossy white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP016902 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP032302 White Metallized Polypropylene Label Products 3M™ White Metallized Polypropylene Label Products FP032302, FP032302W and FP032305 are a white opaque material that offers excellent durability and opacity. These label products utilize 3M™ Adhesi.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP032302W White Metallized Polypropylene Label Products 3M™ White Metallized Polypropylene Label Products FP032302, FP032302W and FP032305 are a white opaque material that offers excellent durability and opacity. These label products utilize 3M™ Adhesi.. |
|||
Thickness | 58.4 microns | 2.30 mil | Total; ASTM D3652 |
3M Scotch® 5912 Cellophane Tape Scotch® Tape 5972 is a transparent cellophane tape designed for light-duty packaging applications. It is typically used for bag closing, temporary holding, and L-clip applications that do not put s.. |
|||
Thickness | 58.4 microns | 2.30 mil | Total; ASTM D3652 |
3M Scotch® 610 Cellophane Film Tape Scotch® Cellophane Film Tape 610 is a high performance, transparent cellophane film tape featuring a high tack adhesive system. This product offers excellent adhesion, dispensing and handling prope.. |
|||
Thickness | 58.4 microns | 2.30 mil | Total; ASTM D3652 |
3M Scotch® 690 Colored Film Tape Scotch® Tape 690 is a colored film tape featuring a durable, moisture- and chemical- resistant 3M™ Paklon™ film backing with a rubber resin adhesive. This decorative film is excellent for various.. |
|||
Thickness | 58.4 microns | 2.30 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Thickness | 58.4 microns | 2.30 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP4090-S1 High Temperature Protective Coating, Silicone |
|||
Thickness | 58.4 microns | 2.30 mil | |
3M 9552 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP016903 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP02450N Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3800, which is an ultra removable acrylic designed t.. |
|||
Thickness | 58.4 microns | 2.30 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
Thickness | 58.4 microns | 2.30 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
Thickness | 58.4 microns | 2.30 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Thickness | 58.4 microns | 2.30 mil | |
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M 7980 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FV022702 White Vinyl Label Products 3M™ White Vinyl Label Products FV022702 and FV022705 are flexible and conformable materials that offer durability and moisture resistance. The polymerically plasticized nature of this soft flexible.. |