Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 503 microns | 19.8 mil | Typical; ASTM D374 |
DuPont™ Nomex® N196 Paper, 20 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |