Physical Properties Metric English Comments
Thickness 445 microns
17.5 mil
Total; ASTM D3652
3M 436/Silver Damping Foils
Low temperature vibration dampingInformation provided by 3M
Thickness 445 microns
17.5 mil
ASTM D3652
3M 436 Vibration Damping Tape
3M™ Vibration Damping Tapes are low temperature 3M™ Viscoelastic Damping Polymers Tape 830 coated on the dead soft aluminum foil constraining layer. They have pressure sensitive properties and are..
Thickness 445 - 521 microns
17.5 - 20.5 mil
Overall
Arlon R31961R019 0.019" (0.483 mm) Uncured Silicone Rubber with Fiberglass Substrate