Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 419 microns | 16.5 mil | |
Hexcel® HexForce™ 1568 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 419 microns | 16.5 mil | |
Hexcel® HexForce™ 7594 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 419 microns | 16.5 mil | |
Hexcel® HexForce™ SGP370-8H Carbon Fabric Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper.. |
|||
Thickness | 419 microns | 16.5 mil | overall; Arlon SQA-TMS-003 |
Arlon 51106R015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 419 microns | 16.5 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51986R015 0.0165" (0.419 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater substrateAppearance: Red colo.. |
|||
Thickness | 419 microns | 16.5 mil | overall; Arlon SQA-TMS-003 |
Arlon I51576R015 Silicone Rubber/Fiberglass/Alloy Laminate Top layer of side 2: alloy 600 foil; Bottom layer of side 2: cured silicone rubber; Substrate is 7628 fiberglass; Side 1: cured silicone rubber |
|||
Thickness | 419 microns | 16.5 mil | Overall; Arlon SQA-TMS-003 |
Arlon P29514R015 0.0165" (0.419 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassProduct Advatages:Flexibility: Silicone rubber resists damage due to vibration, frame movement under loa.. |
|||
Thickness | 419 microns | 16.5 mil | side 1 silicone; Arlon SQA-TMS-003 |
Arlon 49283R040 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil polyethylene; Side 1: cured silicone rubber; Substrate: 1681 Fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 419 microns | 16.5 mil | overall; Arlon SQA-TMS-003 |
Arlon 51146R015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 419 microns | 16.5 mil | overall; Arlon SQA-TMS-003 |
Arlon 51276R015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |