Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 394 microns | 15.5 mil | |
Hexcel® HexForce™ 7547 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 394 microns | 15.5 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51576B015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate.. |
|||
Thickness | 394 microns | 15.5 mil | Side 1, Uncured Layer; Arlon SQA-TMS-003 |
Arlon R35928R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |
|||
Thickness | 394 microns | 15.5 mil | Overall; Arlon SQA-TMS-003 |
Arlon R35948R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberThis data re.. |
|||
Thickness | 394 microns | 15.5 mil | Overall; Arlon SQA-TMS-003 |
Arlon R36338R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Uncured Silicone Rubber Substrate: Style 7628 FiberglassSide 2: Cured Silicone RubberAppearan.. |
|||
Thickness | 394 microns | 15.5 mil | overall; Arlon SQA-TMS-003 |
Arlon 51228R015 Silicone Rubber/Fiberglass Laminate Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 394 microns | 15.5 mil | side1/uncured; Arlon SQA-TMS-003 |
Arlon 51228R025 Silicone Rubber/Fiberglass Laminate Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 394 microns | 15.5 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51576W015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: White silicone gum on glass fabricThis data re.. |
|||
Thickness | 394 - 470 microns | 15.5 - 18.5 mil | Overall |
Arlon R33826R017 0.017" (0.432mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 394 microns | 15.5 mil | Overall; Arlon SQA-TMS-003 |
Arlon R35928R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |