Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 31580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on an HDPE Carrier
(discontinued * Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Side 1 |
Arlon 31580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on an HDPE Carrier
(discontinued * Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 28601M015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Tan gum on glass fiber fabricThis data represents typical values for the production material. The data .. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 28601W015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Product Use: Flexible Heater InsulationAppearance: White silicone gum on fiberglass with polymer release linersThis.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 30570XA015 0.015" (0.381mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Gray silicone gum on polymer linerThis data represents typical values for the production material. Th.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Side 1 |
Arlon 30570XA015 0.015" (0.381mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Gray silicone gum on polymer linerThis data represents typical values for the production material. Th.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 49576R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 49581R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 51570R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 51571XC015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 51580R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 51586X015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of,.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 51589R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of,.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 51591R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis data .. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 51601W015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: White silicone gum on fiberglass with polymer release linersThis .. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon R32481R014 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon R32959R020 0.015" (0.381 mm) Primerless Traction Motor Tape with Fiberglass Substrate Design/Construction:Side 1: Layer-on-LayerAppearance: Red silicone gum on glass fabricThis data Represents typical values for the production material. The data should not be used to write, or in pla.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon R34066X015 0.015" (0.381 mm) Cured Silicone with Fiberglass Substrate Design/Construction:Side 1: Platinum Cured SiliconeSide 2: Peroxide Catalyzed Silicone Appearance: Gray silicone gum on fiberglass clothThis data Represents typical values for the production materia.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Side 1 |
Arlon 30580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The d.. |
|||
Thickness | 343 microns | 13.5 mil | Total; ASTM D3652 |
3M 435/Silver Damping Foils Low temperature vibration dampingInformation provided by 3M |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 44576XB015 0.015" (0.381 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Gray silicone gum and rubber on fiberglass clothThis data represents typical values for the production ma.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 51344R015 0.015" (0.381 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-Cured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to .. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 51571XA015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Gray silicone gum on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 51586B015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Black silicone gum and rubber on fiberglass clothThis data Represents typical values for the production m.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 51970R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, or .. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 51971R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data .. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon R33991R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 30600R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis da.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Side 1 |
Arlon 30600R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis da.. |
|||
Thickness | 343 - 419 microns | 13.5 - 16.5 mil | Overall |
Arlon 44406X015 0.015" (0.381 mm) Platinum Cured Silicone/Peroxide Catalyzed Silicone Design/Construction:Side 1: Platinum Cured SiliconeSide 2: Peroxide Catalyzed SiliconeAppearance: Gray silicone gum on fiberglass clothThis data represents typical values for the production material.. |