Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 305 microns | 12.0 mil | |
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
Thickness | 305 microns | 12.0 mil | |
Rogers Corporation Poron® 4790-92-30012 P Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced Extra soft, slow rebound with a very low closure force. Available with thickness of 0.012" (0.30 mm).Features and Benefits of PORON Products: Excellent compression set resistance which enables dura.. |
|||
Thickness | 305 microns | 12.0 mil | Cured Ply |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, T-700 24K Uni-Tape Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Thickness | 305 microns | 12.0 mil | cured laminate, per ply |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 581 Quartz Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Thickness | >= 305 microns | >= 12.0 mil | Side 1 |
Arlon 515880R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wr.. |
|||
Thickness | 305 microns | 12.0 mil | |
Fibre Glast 530 Plain Weave Carbon Fiber Fabric Graphite fibers contain up to 95% carbon and yield the highest tensile strength in the FRP industry. These fibers woven together form graphite fabric. These fabrics offer higher strength and stiffne.. |
|||
Thickness | 305 microns | 12.0 mil | |
Fibre Glast 549 Kevlar® Fabric This was one of the first high strength synthetic fibers to gain acceptance in the reinforced plastic industry. Unlike the previous synthetic reinforcing fibers, Kevlar® has a considerably higher.. |
|||
Thickness | 305 microns | 12.0 mil | |
Hexcel® HexForce™ 328 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Thickness | 305 microns | 12.0 mil | |
Zircar Zirconia ZYK-15 Zirconia Cloth Insulation Zirconia Cloth Type ZYK-15 is a tricot knit cloth nominally 0.012” thick composed of yttria stabilized zirconia fibers. This material offers extreme temperature and chemical resistance in a flexibl.. |
|||
Thickness | 305 microns | 12.0 mil | |
Hexcel® HexForce™ 1188 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 305 microns | 12.0 mil | Nominal |
DuPont™ Nomex® 410 Paper, 12 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Thickness | 305 microns | 12.0 mil | Nominal |
DuPont™ Nomex® 414 Paper, 12 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Thickness | 305 microns | 12.0 mil | |
3M 5959 Outdoor Masking and Stucco Tape 3M™ Outdoor Masking and Stucco Tape 5959 has a high tensile strength backing for pulling through stucco, EIFS and other heavy coatings. Moisture and UV resistant, strong conformable backing. Clean .. |
|||
Thickness | 305 microns | 12.0 mil | Silicone; Arlon SQA-TMS-003 |
Arlon 51044R020 0.020" Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Semi-cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should no.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1 |
Arlon 51580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55572R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1 |
Arlon 55580R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55590R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be us.. |
|||
Thickness | 305 microns | 12.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon Thermabond® 51A50X020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 76.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1 |
Arlon 51344R020 0.020" (0.508 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-Cured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to.. |
|||
Thickness | 305 microns | 12.0 mil | Side 2 |
Arlon 51393R032 0.032" (0.813 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Pad Life: Temperature and time dependentThis data represents typical values for the production material. The data shoul.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1 |
Arlon 51420R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55100R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricT.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55272R028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
Thickness | 305 microns | 12.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 912-10X##-P0 0.012" (0.305 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 12 mil thick, Gray, Rectangular cross-section, Self-fus.. |
|||
Thickness | 305 microns | 12.0 mil | Silicone; Arlon SQA-TMS-003 |
Arlon 91B32R016AC Aluminum Clad Silicone Press Pad with "C-finish" Design/Construction:Side 2: Alloy 1100 H18 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specificatio.. |
|||
Thickness | 305 microns | 12.0 mil | ASTM D3652 |
3M Scotch® 393 General Purpose Cloth Tape Scotch® General Purpose Cloth Tape 393 is a polyethylene coated cloth backing coated with a rubber adhesive for moisture-proofing, duct sealing and general purpose applications.Information provided.. |
|||
Thickness | 305 - 356 microns | 12.0 - 14.0 mil | Overall |
Arlon 44686W013 0.013" (0.330 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber UL Recognition: 220°C per UL Card E54153Appearance: White silicone gum on fiberglassThis data represents typical val.. |