Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | >= 300 microns | >= 11.8 mil | Minimum Web |
GrafTech GRAFCELL® FFP-300 SERIES Flow Field Plate Graphite Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid.. |
|||
Thickness | 300 microns | 11.8 mil | |
Shandong Dongyue Shenzhou New Material Co CHFM 300 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM) Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th.. |
|||
Thickness | 300 microns | 11.8 mil | Nominal |
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Thickness | 300 microns | 11.8 mil | Nominal |
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Thickness | 300 microns | 11.8 mil | |
Hexcel® HexForce™ 7500 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |