Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 31.8 microns | 1.25 mil | |
Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer with enhanced stabilization packageCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use stra.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
M. Holland Company LL104 LLDPE
(discontinued **) Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-144 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 2% vinyl acetate copolymer packaging film resin. Film made from LD-144 offers improved impact strength and heat sealability compared to homopolym.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-306 EVA Film Resin, High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.5% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-312 EVA Film Resin, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 4.6% vinyl acetate copolymer resin for films with good toughness. This resin's low melt index and comonomer content help produce films which exhi.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-318 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-318 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-333 EVA Film Resin, Very High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-333 exhibits superior impact strength, clarity and heat sealability.Applications: Prim.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-336 EVA Film Resin, Clarity, Very High Drawdown
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer blown film resin capable of very high drawdown with excellent clarity.Applications: Very thin heat seal layers; Light.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-768 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low gel 27.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-129 MDPE Cast Overwrap Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-129 can be used in overwrap applications and in push-through .. |
|||
Thickness | 31.8 microns | 1.25 mil | |
LyondellBasell Petrothene® NA285003 Medium Density Polyethylene ApplicationsPETROTHENE NA 285-003 is a medium density polyethylene resin for blown or cast film extrusion. Typical applications include overwrap film. This product exhibits good film optics and hi.. |
|||
Thickness | 31.8 microns | 1.25 mil | 2.2:1 BUR |
LyondellBasell Petrothene® NA334000 Low Density Polyethylene ApplicationsPETROTHENE NA 334-000 is a homopolymer resin specifically engineered for thin film applications. NA 334-000 is know for its consistency, exceptional drawdown and processability. Regulat.. |
|||
Thickness | 31.8 microns | 1.25 mil | 2.2:1 BUR |
LyondellBasell Petrothene® NA336149 Low Density Polyethylene ApplicationsPETROTHENE NA 336 is a homopolymer resin specifically engineered for garment film and dry cleaning bag applications. This resin is also suitable for any application requiring thin gauge.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
LyondellBasell Petrothene® NA340185 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea.. |
|||
Thickness | 31.8 microns | 1.25 mil | Blown, as tested |
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Thickness | 31.8 microns | 1.25 mil | 2:1 BUR; 25 mil die gap |
LyondellBasell Petrothene® NA420000 Low Density Polyethylene ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
Thickness | 31.8 microns | 1.25 mil | 2:1 BUR; 25 mil die gap |
LyondellBasell Petrothene® NA951000 Low Density Polyethylene ApplicationsPETROTHENE NA 951 is a series of homopolymer resins specially designed for industrial and consumer packaging and liner and bag applications. NA 951 has an excellent balance of processab.. |
|||
Thickness | 31.8 microns | 1.25 mil | Cast, as tested |
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Thickness | 31.8 microns | 1.25 mil | Blown, as tested |
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
Westlake DA591 9.0% Ethylene Vinyl Acetate Copolymer Westlake DA591 resin is a 9.0% EVA copolymer designed as a tie layer in multi-layered food packaging film. It has excellent clarity, excellent toughness, good resistance to load deformation, and goo.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
Westlake EF378 Low Density Polyethylene WESTLAKE EF378 is suggested for cast film applications. It has excellent haze and gloss, good strength, good processability, and good heat sealability.Application/UsesDiaper linersGeneral purpose cl.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
Westlake EF412 Low Density Polyethylene WESTLAKE polyethylene EF412 is a low-density polyethylene with very good optical and strength properties. This material is an excellent choice for bakery films and food packaging applications.Applic.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
Westlake Elevate™ EF446 6.0% Ethylene Vinyl Acetate Copolymer Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
Chevron Phillips MarFlex® 7109DJ LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil EXACT™ 3132 Plastomer for Blown Film Applications Product Description: Exact 3132 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3132 is designed for both monolayer and multilayer blo.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
M. Holland Company MAGMA® LL1091-AS LLDPE
(discontinued **) Additives: Medium Antiblock, Medium SlipFeatures: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Thickness | 31.8 - 50.8 microns | 1.25 - 2.00 mil | Average value: 34.9 microns Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |
|||
Thickness | 31.8 microns | 1.25 mil | |
ExxonMobil Escorene® LD-331 EVA Film Resin, Very High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |
|||
Thickness | 31.8 microns | 1.25 mil | |
M. Holland Company MAGMA® LL1092-K LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |