Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 4.83 microns | 0.190 mil | ASTM D3652 |
3M Scotch® 231 Performance Masking Tape Scotch® Performance Masking Tape 231 is a premium high performance crepe paper masking tape designed to perform well in most industrial painting situations, including the use of bake cycles. This s.. |
|||
Thickness | 4.83 microns | 0.190 mil | ASTM D3652 |
3M Scotch® 231A Performance Masking Tape Scotch® Performance Masking Tape 231A is a premium high performance crepe paper masking tape designed to perform well in most industrial painting situations, including the use of bake cycles. This .. |