Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 0.279 microns | 0.0110 mil | cured laminate, per ply |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Thickness | 0.280 microns | 0.0110 mil | 3000 rpm |
Dow SiLK™ I300 280 Semiconductor Dielectric Resin SiLK™ I300 280 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 280 is compatibl.. |