Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 686 - 787 microns | 27.0 - 31.0 mil | Overall |
Arlon 55578XC028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 686 - 787 microns | 27.0 - 31.0 mil | Overall |
Arlon 55578XD028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers Appearance: Gray silicone gum and/or rubber on fiberglass clothThis data Represents typical values for the production ma.. |
|||
Thickness | 737 - 787 microns | 29.0 - 31.0 mil | Overall |
Arlon 55579R028M 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured layer on top of a cured layer on one side This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 711 - 787 microns | 28.0 - 31.0 mil | Overall |
Arlon 55589W028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or.. |
|||
Thickness | 711 - 787 microns | 28.0 - 31.0 mil | Overall |
Arlon 55596R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of,.. |
|||
Thickness | 686 - 787 microns | 27.0 - 31.0 mil | Overall |
Arlon 55606R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl.. |
|||
Thickness | 635 - 787 microns | 25.0 - 31.0 mil | Overall |
Arlon 55571R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 737 - 787 microns | 29.0 - 31.0 mil | Overall |
Arlon R33089X028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 508 - 787 microns | 20.0 - 31.0 mil | Range of Thicknesses Available |
Rogers Corporation Bisco® EC-2040 Conductive Silicone Base Polymer: SiliconeFiller: Nickel-GraphiteApplications: Silicone EMI ShieldsThickness: 0.020 inches and 0.031 inchesInformation provided by Rogers Corporation. |