Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology EXXTRAL® plus PVD Coating Key Characteristics: high hardness, very good oxidation resistance, low thermal conductivityPrimary Applications: machining of hardened steel and thicker steel sheets; excellent chemical resistance;.. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology EXXTRAL® rose PVD Coating Key Characteristics: high hardness and elasticity, low friction, high oxidation resistancePrimary Applications: excellent for stainless steel and nickel-based high temperature alloys; hard and copy .. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology EXXTRAL® silver PVD Coating Key Characteristics: high hardness, good oxidation resistance, low frictionPrimary Applications: machining of abrasive or sticking materials (stainless steel, cast iron, Si-rich Al-alloys); machinin.. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology SISTRAL® AlTiN PVD Coating Key Characteristics: extreme wear resistance at high temperature, excellent oxidation resistancePrimary Applications: excellent choice for cutting under extreme conditions (hard abrasive materials, .. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology SUPRAL TiAlN PVD Coating A TiAlN-based hard coating, especially developed for drilling under extreme conditions.Information provided by Eifeler Coatings Technology |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology TiCN PVD Coating Key Characteristics: high hardness excellent abrasive wear resistance, enhanced toughnessPrimary Applications: machining of difficult to machine alloy steels; high performance cutting where moderate.. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology TiN PVD Coating Key Characteristics: standard all purpose coatingPrimary Applications: machining / cutting of iron based material; metal forming; plastic molding of highly abrasive plastics; orthopedic instrumentat.. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology VARIANTA® TiAlN PVD Coating Key Characteristics: high hardness, very good oxidation resistancePrimary Applications: coating for a wide range of carbide, cermet and high speed steel tools; machining of cast iron and nickel base.. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology VARIANTIC® TiAlCN PVD Coating Key Characteristics: low friction, good oxidation resistancePrimary Applications: coating for a wide range of carbide, cermet and high speed steel tools; machining of all types of steel under dry as.. |
|||
Thickness | 1.00 - 4.00 microns | 0.0394 - 0.157 mil | |
Eifeler Coatings Technology WC/C PVD Coating Key Characteristics: high lubricity, low tendency for adhesive wearPrimary Applications: on top of hard coatings for reduction of friction; precision components: automotive, aerospace, medicalInform.. |
|||
Thickness | 1.00 - 4.00 microns | 0.0394 - 0.157 mil | |
Eifeler Coatings Technology ZrCN PVD Coating Key Characteristics: decorative color, good wear and corrosion resistancePrimary Applications: machining of cast aluminum, brass, copper, bronze, non-alloyed aluminum; machining of fiberglass, nylon.. |
|||
Thickness | 1.00 - 4.00 microns | 0.0394 - 0.157 mil | |
Eifeler Coatings Technology ZrN PVD Coating Key Characteristics: decorative color, good wear and corrosion resistancePrimary Applications: cast aluminum and generally non-ferrous materials machining; machining of fiberglass, nylon and most po.. |
|||
Thickness | 0.100 - 4.00 microns | 0.00394 - 0.157 mil | Coating Thickness |
BACT DLC Diamond-Like Coating DLC (a-C:H). This coating provides the highest hardness and abrasion resistance of the BACT products. Typical applications include high wear environments involving seals, molds, metal forming, and.. |